About six percent of what arrives at our yard cannot be put back into service. This is the story of that six percent, which is the only part of our operation where something gets destroyed.
Three strikes
A bottle gets three independent assessments before anyone is permitted to shred it: at intake, after washing, and at the test cell. Three different people have to agree that it is finished. This sounds excessive. It exists because the easiest way to destroy value in this business is to condemn a container that was fine.
The line
- Stripped - valve, lid, gaskets and labels removed, each to its own stream.
- Separated - cage and pallet leave for reuse or for the steel mill.
- Granulated - the bottle is shredded to flake in a knife mill.
- Washed and floated - contamination separated by density in a float tank.
- Dried and bagged - clean natural or mixed-colour HDPE regrind, sold by the gaylord.
Where the material goes
Our regrind goes to extruders making corrugated pipe, plastic lumber, agricultural drainage and non-food rigid goods. It does not go back into food-contact bottles, which require virgin resin, and we are explicit about that rather than letting the word recycled do vague work.
Why the number matters
Six percent is a target, not a brag. Every point we push it down is a container that stayed a container. The granulator is the most environmentally virtuous machine in the building and we would still be delighted to run it less.