Skip to content
Totes Nation
Dallas, TX · Est. 2009Get a quote
What it is made of

Four materials. Wildly different lives.

The bottle is the decision. Everything else - cage, pallet, valve - is logistics. Here is what each material tolerates, where it fails and what it costs you to be wrong.

Fast lane

Compatibility check

Send the SDS or just name the product. Compatibility checks are free and take us minutes.

Yard & office9003 Governors Row, Dallas, TX 75247hello@totesnation.com

A working business mailbox - we reply here.

US or Canadian number, 10 digits including area code

Two-letter code or full name

US ZIP (75247) or Canadian (M5V 3L9)

Whole units, 1 to 100,000

Please describe it in words - links are not accepted.

No phone tag. A human replies from Dallas within one business day.
The four

Material properties side by side.

PropertyHDPEPolypropyleneFluorinated HDPE316L stainless
Typical useGeneral liquid serviceValves, closures, hot fillSolvents, fuels, aromaticsAggressive and sanitary
Max continuous temp140 F / 60 C180 F / 82 C140 F / 60 C600 F+ / 315 C+
Min temp-40 F32 F (brittle below)-40 FCryogenic
UV resistancePoor without additivePoorPoorExcellent
Permeation (hydrocarbons)HighModerateVery lowNone
Impact resistanceExcellentFair when coldExcellentExcellent
Typical service life5-8 yearsn/a (component)5-8 years20-40 years
Relative cost$$$$$$$$$
The one people underestimate

Permeation is invisible until it is not.

Untreated HDPE is semi-permeable to hydrocarbons. A tote of xylene stored for six months loses product, gains a swollen bottle wall and fills the warehouse with vapor nobody can locate. Nothing leaks. Nothing is on the floor. The container is simply breathing.

Fluorination fixes this by reacting fluorine gas with the inner surface to form a barrier layer a few micrometers thick. It typically reduces permeation by well over 90 percent at a fraction of the cost of stainless.

If your product has a strong smell and a low molecular weight, assume permeation is a factor and ask us before you store it in plain HDPE.

Fluorinated & stainless options
Red flags for plain HDPE
  • Aromatic solvents: xylene, toluene, benzene
  • Ketones: acetone, MEK
  • Chlorinated solvents of any kind
  • Fuels and fuel additives
  • Essential oils and strong fragrances
  • Anything stored above 120 F for long periods
  • Anything stored outdoors in direct sun for years
Cage, pallet, hardware

The other materials in the stack.

ComponentMaterialWhyWatch for
CageGalvanized tubular steelStrength and stackabilityRust at weld joints, bent bottom rail
Pallet - steelGalvanized steelDurable, lowest profileCorrosion in wet service
Pallet - compositeHDPE over steelExport friendly, no ISPM-15 issueCracking at fork pockets
Pallet - woodHardwoodCheapISPM-15 required for export, absorbs spills
Valve bodyPolypropyleneChemical resistance, costCold brittleness, UV
Valve seatEPDM or FKM (Viton)Seal against productWrong elastomer for the cargo
LidHDPEMatches bottleVented vs solid confusion
Material questions

Asked by engineers and buyers alike.

01Is recycled HDPE used in your bottles?

Not in rebottled units - those are virgin resin for food-contact compliance. Our recovered material goes to extruders making pipe, lumber and non-food rigid goods. See recycling and regrind.

02How long does an HDPE bottle really last?

Indoors, five to eight years in liquid service. Outdoors in Texas sun, as little as three. UV is the dominant ageing factor, not chemistry.

03Does fluorination wear off?

The barrier layer is chemically bonded and does not wash out, but aggressive scrubbing or harsh caustic cycles degrade it over many washes. We note fluorinated units and wash them accordingly.

04Why 316L rather than 304?

Molybdenum. 316L handles chlorides and many acids far better. For food, pharma and most chemical service, 316L is the standard and 304 is a compromise.

Chemical resistance

A longer compatibility reference.

Indicative ratings at ambient temperature and ordinary dwell times. Elevated temperature degrades every rating below, usually by one step.

This table is a starting point for a conversation, not a specification. Send us the SDS and we will check concentration, temperature and dwell properly - it takes minutes and costs nothing.
ChemicalHDPEPPFluorinated HDPE316LNote
Acetic acid 10%ExcellentExcellentExcellentGoodDilute only
Ammonium hydroxideExcellentExcellentExcellentExcellentVents - use a vented lid
Citric acidExcellentExcellentExcellentExcellentFood service common
Ethylene glycolExcellentExcellentExcellentExcellentCoolant service
Ferric chlorideExcellentExcellentExcellentPoorChlorides attack stainless
Hydrochloric acid 30%GoodGoodGoodPoorChlorides again
Hydrogen peroxide 35%GoodFairGoodGoodNeeds venting and clean surfaces
Isopropyl alcoholGoodGoodExcellentExcellentPermeates slowly
MethanolGoodGoodExcellentExcellentPermeation over long dwell
Mineral spiritsFairGoodExcellentExcellentClassic permeation case
Nitric acid 10%GoodGoodGoodExcellentConcentration matters a lot
Phosphoric acid 85%ExcellentExcellentExcellentGoodCommon in ag chemistry
Sodium hypochlorite 12.5%GoodGoodGoodPoorDegasses - vent it
ToluenePoorFairGoodExcellentFluorinate or go stainless
Urea solution (DEF)ExcellentExcellentExcellentExcellentCleanliness is the real issue
Ageing

How HDPE actually fails.

Four mechanisms, in the order they matter. Only one of them is about chemistry.

MechanismTriggerVisible signReversible?
UV photo-oxidationSunlight over months and yearsChalky surface, loss of flexibility, crazingNo
Environmental stress crackingStress plus a surfactant or solventFine cracks at stress pointsNo
Swelling and softeningSolvent absorptionPanel distortion, soft wall, odourPartly, with long airing
Thermal deformationSustained heat above 140 FPermanent shape changeNo
Temperature

What each material does when it gets hot or cold.

Service temperature is where material selection usually goes wrong, because the specification sheet quotes a maximum that assumes no load and no pressure.

The practical limit on a filled HDPE IBC is lower than 140 F, because hydrostatic load and heat combine. Hot-fill applications need a conversation before you order.
MaterialContinuous minContinuous maxBrief excursionWhat failure looks like
HDPE-40 F140 F160 F unpressurisedSoftening, bulging, loss of stacking strength
Polypropylene32 F180 F200 FBrittle fracture when cold, creep when hot
304 stainless-320 F800 FHigherEssentially none in this range
316 stainless-320 F800 FHigherEssentially none in this range
Carbon steel, lined-20 F250 FLining dependentLining blisters and lifts
EPDM seals-40 F250 F300 FHardening, then leaking
Viton / FKM seals-15 F400 F450 FStiffening when cold
PTFE seals-320 F500 F550 FCold flow under sustained load
Galvanized cage-40 F390 FHigherZinc coating degrades above 390 F
Identification

Telling the plastics apart without a lab.

Useful when somebody hands you an unmarked container. None of this is definitive, but together it will get you to the right answer.

Check the moulded recycling mark on the base or the neck before doing anything else. It is there on almost every container made since the 1990s.
TestHDPEPolypropylenePVCHDPE vs PP verdict
Float in waterFloatsFloatsSinksNeither sinks
Float in 50% alcoholSinksFloatsSinksSeparates the two
Fingernail scratchMarks easilyMarks lessHardHDPE is softer
Flex at the cornerWaxy, bends whiteSpringy, hingesBrittlePP hinges without stress whitening
Sound when tappedDullSlightly brighterSharpSubtle, needs practice
Surface feelWaxySlightly slickHard, smoothHDPE feels waxier
Recycling mark2 or PE-HD5 or PP3 or PVCCheck the mark first, always
Burn testBlue flame, candle smellBlue flame, less smokeSelf-extinguishing, acridDo this outdoors only, if at all
Permeation

The quiet problem with plastic containers.

HDPE is not a perfect barrier. For most cargoes this is irrelevant, but for a handful it decides whether plastic is viable at all.

Fluorination is a surface treatment applied to the inside of a bottle at manufacture. It cannot be applied to a used container, so it has to be specified at the point of purchase.
CargoPermeation through HDPEEffectWhat to use instead
Water, brines, most aqueousNegligibleNoneHDPE is correct
GlycolsNegligibleNoneHDPE is correct
Mineral oilsLowSlight weight loss over yearsHDPE is fine
Gasoline and light fuelsSignificantLoss, odour, swellingFluorinated HDPE or steel
Aromatic solventsHighSwelling, wall weakeningSteel or stainless
Chlorinated solventsHighSwelling, rapid failureSteel or stainless
Essential oils and fragrancesModerateOdour permanently absorbedStainless, or a dedicated unit
Agricultural actives in solventModerateContainer cannot be reusedFluorinated HDPE
Next move

Free compatibility check.

Send the SDS. We will tell you which material survives your product and which one quietly fails.

Reference · on every page for a reason

The numbers people ask us for twice a week.

Specifications, capability and contact details in one block, so you never have to go hunting for them from wherever you happen to be on this site.

Totes Nation at a glance
Founded2009
Head office & yardDallas, TX
Street address9003 Governors Row
ZIP75247
People71
Yard size9 acres, 11 dock doors
Wash capacity1,200 units/day
States served48
Quote turnaround1 business day
PhoneNone - email only
Everything we do
  • Buy used IBC totes, drums, cages and pallets nationwide
  • Sell reconditioned, rebottled and food grade containers
  • Hot caustic wash with counter-current triple rinse
  • Food grade protocol in an isolated circuit with swab verification
  • UN 31HA1 leak and pressure testing with reconditioner marking
  • Cage straightening, revalving and full hardware replacement
  • Freight booking: partial, consolidated and full truckload
  • Managed container fleet programmes from 150 units
  • On-site granulation into clean HDPE regrind
  • Custom fabrication, plumbing, branding and upcycled builds
Office & dock hours
Monday - Thursday7:00 AM - 5:00 PM CT
Friday7:00 AM - 3:00 PM CT
Saturday8:00 AM - 12:00 PM CT (dock pickups only)
SundayClosed

Write to us

Every message is read by a person in Dallas and answered within one business day.

Quick specification

Container fast reference.

Nominal figures for the containers we stock. Gross weights assume water at 8.345 lb per gallon - multiply by your product specific gravity.

Full dimensions, clearances, thread data and UN codes are in Sizes & Specs.
ContainerCapacityFootprintHeightTareGross (water)Outlet
Caged IBC, standard275 gal / 1,041 L48" x 40"46"125 lb2,419 lbS60x6
Caged IBC, tall330 gal / 1,249 L48" x 40"53"148 lb2,902 lbS60x6
Caged IBC, low profile180 gal / 681 L48" x 40"35"104 lb1,606 lbS60x6
Caged IBC, compact120 gal / 454 L40" x 32"34"78 lb1,079 lbS60x6
Stainless IBC350 gal / 1,325 L48" x 42"51"320 lb3,241 lbNPT / TC
Poly drum, tight head55 gal / 208 L23" dia.35"22 lb481 lb2" NPS
Steel drum, tight head55 gal / 208 L23" dia.34"38 lb497 lb2" NPS
Asked from every page

Five answers that apply wherever you are.

01What does a used IBC tote actually cost?

It depends on grade, quantity and your distance from Dallas, and freight is often the biggest single variable. Grade C units are a fraction of Grade A, rebottled sits near the top, and food grade is priced by scarcity of documented stock. Send a quantity and a zip code and you get a landed number, not a range. The pricing guide shows the bands we work in on the buy-back side.

02How fast can I get containers?

Stock units leave the yard in two to three business days, rebottled in two to five, food grade in three to seven. Add transit: next day in the Texas triangle, two to three days through the Midwest and Southeast, three to five to the coasts. Full lane detail is on the locations page.

03Will you buy the empties I already have?

Yes, in all 48 contiguous states, including damaged units and mixed unsorted lots. Freight is netted into the price so you see one clear per-unit number, and within 150 miles of Dallas collection is free. Details on we buy your totes.

04How do I know what grade I need?

Tell us the cargo rather than the grade. We publish a written grading standard and we will usually recommend a cheaper grade than people ask for, because most jobs do not need appearance. The Tote Matchmaker encodes the same conversation in four questions.

05Why is there no phone number anywhere on this site?

Because we have never had one. Written answers give you a record, a quote you can forward and a grade you can hold us to, and they are a large part of why every request gets answered within one business day. The form on this page reaches the same people a phone line would have.